抽象的な

An eco friendly method of total iron estimation in HBI /DRI

D.G.Annapurna


Metallization of Hot briquetted iron (HBI) and Direct reduced iron (DRI) plays key role in Steel making process. Total Iron estimation is a part of Metallization, conventionally it is estimated by dissolving sample in Hydrochloric acid (HCl) to convert Fe into Ferric (III) followed by Ferrous F (II) with Stannous chloride. Mercuric chloride is added in this process which is hazardous in nature causes impact to environment. In this new Eco friendly method of Total Iron estimation in HBI/DRI where sample is dissolved in dilute sulfuric acid (H2SO4) to convert Fe to Fe (II) directly. The results are matching for both the methods. This new method is applicable to HBI/DRI samples where metallization is >90%. Not applicable to IronOxides.


免責事項: この要約は人工知能ツールを使用して翻訳されており、まだレビューまたは確認されていません

インデックス付き

  • キャス
  • Google スカラー
  • Jゲートを開く
  • 中国国家知識基盤 (CNKI)
  • サイテファクター
  • コスモスIF
  • 電子ジャーナルライブラリ
  • 研究ジャーナル索引作成ディレクトリ (DRJI)
  • 秘密検索エンジン研究所
  • ICMJE

もっと見る

ジャーナルISSN

ジャーナル h-インデックス

Flyer

オープンアクセスジャーナル